Although the quality of enameled wire depends to a large extent on the quality of raw materials such as paint and wires and the objective conditions of machinery and equipment, if a series of issues such as baking, annealing, and vehicle speed are not taken seriously in operation and their interrelationships are not understood, without mastering the operating techniques, not conscientiously doing patrol work and parking arrangements, and not doing a good job of process hygiene, no matter how good the objective conditions are, you will not be able to produce good enameled wire. Therefore, the decisive factor for good enameled wire is people and their sense of responsibility for their work.

 

 

1. Before starting the catalytic combustion hot air circulation enameling machine, the fan should be turned on to circulate the air in the furnace at a slow speed. Preheat the furnace and catalytic zone with electric heat so that the temperature of the catalytic zone reaches the specified ignition temperature of the catalyst.

 

2. "Three Diligences" and "Three Inspections" in production operations.

 

The paint film is measured once an hour, with the zero position calibrated before each measurement. When measuring the line, keep the micrometer gauge at the same speed as the line, and measure the large wire in two mutually perpendicular directions.

Regularly observe the back-and-forth alignment and tension, making timely corrections as needed. Ensure that the lubricating oil is properly applied.

 

Frequently check the surface for graininess, paint peeling, and other undesirable phenomena in the enameled wire during the coating process. Identify the cause and correct it immediately. For defective products on the line, remove the axle in a timely manner.

Check the operation by ensuring all running parts are functioning normally. Pay attention to the tightness of the pay-off shaft to prevent rolling, breakage, and thinning of the wire diameter.

Monitor the temperature, speed, and viscosity according to process requirements.

 

During the production process, continuously check that the raw materials meet the technical requirements.

 

3. In the production operation of enameled wire, attention should also be paid to the problems of explosion and fire. The following types of fire situations occur:

First, the entire furnace is on fire, which is often caused by excessive vapor density across the cross section of the furnace or excessively high furnace temperature.

Second, by excessive amounts of paint on several wires when threading, causing several wires to catch fire.

To prevent fire, we must first strictly control the temperature of the process furnace, and secondly, make the furnace ventilated smoothly.